Mar 31, 2017
It is carried out in the zinc wire replacement box by replacing the gold with the zinc wire from the gold-containing liquid. The technical operation is as follows:
1. Zinc wire added zinc wire should be loose, evenly spread to the box on the screen, can not stay through the hole. And each class must add the right amount of zinc wire to supplement consumption. In order to keep the zinc wire loose, usually should always mention the handle up and down jitter, to promote the surface attached to the zinc wire gold sink to the bottom of the box, so that zinc wire exposed fresh surface, and timely discharge of hydrogen, to facilitate the replacement process can be carried out smoothly.
2. Production inspection production should always observe whether the abnormal, if the zinc surface appears white precipitate, should be appropriate to add cyanide; found zinc wire surface was yellow and red, indicating high copper content, should take timely measures to discharge copper interference ; If the zinc wire surface is covered with mud, indicating that too much suspended solids in your liquid, should strengthen the purification operations. In addition, you can also add a new zinc wire surface to determine whether the reaction rate is normal.
3. Extraction of gold mud before the extraction of gold mud should first stop the supply of liquid, and then extract the gold mud. It is best to stop the supply of liquid to the box for the poor liquid, so that the top of the box without the replacement of the liquid, when the box filled with liquid, to be clarified for a while and then extract the gold mud.
Copyright © Shijiazhuang CanChun Metal Products Trade Co., Ltd. All Rights Reserved.| Sitemap
Online Services